If a PCB photoimageable system fails to develop cleanly, does that mean the resin’s molecular weight is too high?

UpdateTime:2026-11-16

Q. If a PCB photoimageable system fails to develop cleanly, does that mean the resin’s molecular weight is too high?

A. The high-molecular-weight tail of the resin’s molecular weight distribution may contribute to incomplete development. Also check the resin’s acid value, exposure and prebake conditions, film thickness, and development settings. Review the full molecular weight distribution and compare formulations under the same processing conditions to help identify the cause.